Short answer: Austempered ductile iron is ductile iron heat-treated to a bainitic matrix, delivering high strength with useful toughness and wear resistance at lower cost than forged steel – the process is in our Metal Heat Treatment Guide and the base material in our Ductile Iron Guide.
At a Glance

What Austempering Does
The part is austenitised then quenched into a salt bath and held to form bainite, avoiding brittle martensite; the general cycle is in our Metal Heat Treatment Guide.
ADI Grades and Properties
Grades state minimum tensile strength from about 900 to 1400 MPa, traded against elongation; the base ductile grades are in our Ductile Iron Guide.
ADI vs Forged Steel
ADI offers near-forged strength with better castability and damping; the route comparison is in our Cast vs Forged Guide.
Where ADI Is Used
Gears, crankshafts, suspension parts and wear components; the performance context is in our Cast Iron vs Steel Guide and duty in our Mining Guide.
Process Control
Bath temperature and hold time control the bainite; consistency is checked per our Quality Inspection Guide.
Ordering Notes
Specify ADI grade, base iron and drawing; price with our Price Quotation Guide.
Get a Quote
Tell HXSCO your requirements and we will respond with a competitive quote and lead time.
Domande frequenti
Austempered ductile iron, a bainitic high-strength iron.
Grades range from about 900 to 1400 MPa tensile.
Often, for gears and wear parts.
Yes, but usually machined before austempering.
Yes – to grade and drawing.
Get an ADI Quote
HXSCO supplies austempered ductile iron castings to ADI grades with heat-treatment and inspection certificates. Send your drawing for a quote.