Short answer: Common casting defects – gas porosity, shrinkage, cold shuts, sand inclusions and cracks – come from gating, melting or mould issues and are prevented process control and inspection, as covered in our Metal Casting Guide 그리고 Quality Inspection Guide.
At a Glance

Why Casting Defects Happen
Defects trace to melt chemistry, mould condition, gating and cooling; the process stages are in our Metal Casting Guide.
Porosity and Shrinkage
Gas porosity comes from trapped gas, shrinkage from poor feeding; both are found by sectioning and NDT; see our Quality Inspection Guide.
Cold Shuts and Misruns
Low pour temperature or slow filling freezes the metal before it joins; gating design and superheat are the fix, with the route in our Cast vs Forged Guide.
Inclusions and Surface Defects
Sand inclusions and scabs come from mould erosion; surface care is in our Surface Treatment Guide.
Cracks and Distortion
Residual stress and uneven cooling crack or warp castings; heat treatment can relieve stress per our Metal Heat Treatment Guide.
Inspection and Prevention
Layered inspection and documented process control prevent recurrence; third-party checks are in our Third-Party Inspection Guide and documents in our Mill Test Certificate Guide.
Get a Quote
Tell HXSCO your requirements and we will respond with a competitive quote and lead time.
자주 묻는 질문
Small gas holes trapped during solidification.
Proper risers, chills and feeding.
Metal cooling before two streams fuse.
Visual, sectioning, X-ray and ultrasonic methods.
Yes – see our quality inspection guide.
Source Quality Castings
HXSCO supplies inspected castings with foundry and third-party certificates. Send your drawing and quality requirements for a quote.